Technical Specification

Find Technical Data of our all ACID PROOF Mortars, Bricks - Tiles, as follow :

  FURANE Phenolic K - Silicate Cnsl Sulphur Epoxy Polyester Bricks
 Colour Black Black Off White Black Black Off White Off White Red / White
 Ratio 
 ( Solution : Powder )
1:3 1:3 1:3 1:3 Hotmelt 1:5 1:5 --
 Compressive
 Strength ( kg/cm2 )
350 350 150 280 250 500 500 700
 Flexural
 Strength ( kg/cm2 )
75 75 40 75 70 150 150 200
 Bond Strength
 ( kg/cm2 )
10 10 05 10 10 10 12 --
 Water Absorption
 ( max % )
01 01 18 * 01 01 01 01 02
 Temperature
 Resistant ( max °C )
170 170 900 190 90 90 90 900
 Self Life @ 27 °C ** 60 days 45 days 365 days 90 days Life Time 90 days 90 days Life Time
 * Absorption of Toluene.
 ** @ 27 °C in seal pack Drums and Bags under covered shed.